Abstract
Potassium-ion batteries (KIBs) represent one of the most promising alternatives to lithium-ion batteries (LIBs) considering the potential low cost and abundant potassium resource. In this work, we demonstrate a core-shell structured sponge cathode for KIBs, where amorphous V2O5 uniformly coats on carbon nanotube (CNT) sponge via atomic layer deposition (ALD). The V2O5@CNT sponge shows several advantages as cathode: (1) the three-dimensional (3D) conductive network of CNT sponge offers a fast electron transport pathway, (2) the porous nature and high surface area of CNT sponge enables enough access for electrolyte to V2O5, (3) the amorphous structure of V2O5 offers a fast kinetics upon K-ion insertion/deinsertion. The V2O5@CNT sponge cathode delivers a high capacity of 206 mA h/g and moderate cycling and rate performance in common carbonate-based electrolyte system.
| Originalsprache | Englisch |
|---|---|
| Seiten (von - bis) | 344-349 |
| Seitenumfang | 6 |
| Fachzeitschrift | Journal of Materiomics |
| Jahrgang | 5 |
| Ausgabenummer | 3 |
| DOIs | |
| Publikationsstatus | Veröffentlicht - 28 Mai 2018 |
| Extern publiziert | Ja |
UN-Ziele für nachhaltige Entwicklung (SDGs)
2015 einigten sich die UN-Mitgliedstaaten auf 17 globale Ziele für nachhaltige Entwicklung (Sustainable Development Goals, SDGs) zur Beendigung von Armut, zum Schutz des Planeten und zur Förderung des allgemeinen Wohlstands. Hiermit leisten wir einen Beitrag zu folgendem/n Ziel(en) für nachhaltige Entwicklung (SDGs):
-
SDG 7 Erschwingliche und saubere Energie
ASJC Scopus Sachgebiete
- Elektronische, optische und magnetische Materialien
- Oberflächen, Beschichtungen und Folien
- Metalle und Legierungen
Dieses zitieren
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver